High-temperature nanoindentation creep studies on castable and sintered nanostructured low-activation ferritic-martensitic alloys

  • Stony Brook University
  • Bruker Corporation
  • Oak Ridge National Laboratory

Research output: Contribution to journal › Article › peer-review

6 Scopus citations

Abstract

In this article, we present the creep characteristics of two reduced activation ferritic-martensitic steels of identical starting compositions formed by different fabrication routes: a nanostructured ferritic alloy commonly referred to as a castable nanostructured alloy (CNA) and a sintered nanostructured alloy (SNA) variant. Through a series of nanoindentation experiments spanning a temperature range of 25 °C to 650 °C, with a maximum load of 100 mN, we find creep behaviors in the cast and sintered materials to be remarkably similar. The creep stress exponent (n) for CNA and SNA were found to be in the range of 8–35 and the activation volume was ∼14–42b3, underscoring a dominance of dislocation-mediated mechanisms in both alloys. Notably, we observed a decline in the creep stress exponent with increasing temperature, attributable to the heightened influence of thermally activated dislocations. This phenomenon suggests a potential transition in the deformation mechanism towards a thermally activated dislocation climb process, significantly impacting the observed creep behavior.

Original languageEnglish
Article number155804
JournalJournal of Nuclear Materials
Volume611
DOIs
StatePublished - Jun 2025

Keywords

  • Creep
  • Direct current sintering
  • Nanoindentation
  • Sintered nanostructured alloy
  • Stress exponent