Skip to main navigation Skip to search Skip to main content

On the nature of multiple melting in poly(ethylene terephthalate) (PET) and its copolymers with cyclohexylene dimethylene terephthalate (PET/CT)

  • Carlos A. Avila-Orta
  • , Francisco J. Medellín-Rodríguez
  • , Zhi Gang Wang
  • , Dámaso Navarro-Rodrígueza
  • , Benjamin S. Hsiao
  • , Fengji Yeh
  • Center for Research in Applied Chemistry
  • Stony Brook University
  • Universidad Autonoma de San Luis Potosi

Research output: Contribution to journalArticlepeer-review

69 Scopus citations

Abstract

The multiple melting behavior of poly(ethylene terephthalate) (PET) homopolymers of different molecular weights and its cyclohexylene dimethylene (PET/CT) copolymers was studied by time-resolved simultaneous small-angle X-ray scattering/wide-angle X-ray scattering diffraction and differential scanning calorimetry techniques using a heating rate of 2 °C/min after isothermal crystallization at 200 °C for 30 min. The copolymer containing random incorporation of 1,4-cyclohexylene dimethylene terephthalate monomer cannot be cocrystallized with the ethylene terephthalate moiety. Isothermally crystallized samples were found to possess primary and secondary crystals. The statistical distribution of the primary crystals was found to be broad compared to that of the secondary crystals. During heating, the following mechanisms were assumed to explain the multiple melting behavior. The first endotherm is related to the non-reversing melting of very thin and defective secondary crystals formed during the late stages of crystallization. The second endotherm is associated with the melting of secondary crystals and partial melting of less stable primary crystals. The third endotherm is associated with the melting of the remaining stable primary crystals and the recrystallized crystals. Due to their large statistical distribution, the primary crystals melt in a broad temperature range, which includes both second and third melting endotherms. The amounts of secondary, primary and recrystallized crystals, being molten in each endotherm, are different in various PET samples, depending on variables such as isothermal crystallization temperature, time, molecular weight and co-monomer content.

Original languageEnglish
Pages (from-to)1527-1535
Number of pages9
JournalPolymer
Volume44
Issue number5
DOIs
StatePublished - Feb 10 2003

Keywords

  • Copolymers
  • Melting
  • Poly(ethylene terephthalate)

Fingerprint

Dive into the research topics of 'On the nature of multiple melting in poly(ethylene terephthalate) (PET) and its copolymers with cyclohexylene dimethylene terephthalate (PET/CT)'. Together they form a unique fingerprint.