Probing Sources of Capacity Fade in LiNi0.6Mn0.2Co0.2O2 (NMC622): An Operando XRD Study of Li/NMC622 Batteries during Extended Cycling

  • Stony Brook University
  • Brookhaven National Laboratory

Research output: Contribution to journalArticlepeer-review

57 Scopus citations

Abstract

LiNi0.6Mn0.2Co0.2O2 (NMC622) is one of the most promising Li-ion battery cathodes as it delivers high capacity at high potentials. However, high potentials also lead to decreases in capacity retention where the disintegration of the secondary particles has been implicated as a major driving force of this capacity fade. This has been attributed to anisotropic lattice changes and increased microstrain during cycling. To probe how these factors affect capacity fade, Li/NMC622 batteries were cycled from 3 to 4.3 or 4.7 V and probed with operando X-ray diffraction (XRD) over the 1st, 2nd, and 101st cycles. Further characterization with scanning electron microscopy and inductively coupled plasma-optical emission spectroscopy was also performed. The use of operando XRD over many cycles allowed for the collection of detailed structural information in real time over a time frame in which fading can be observed. During the first two cycles, the cells charged to 4.7 V exhibit increased anisotropic lattice changes as compared to the cells charged to 4.3 V. Upon the 101st cycle, when significant fade has been observed, the cells charged to 4.3 and 4.7 V show identical lattice changes to one another, while the 4.7 V charge limit induces more microstrain. This shows that elevated microstrain at high charge limits is a major driver for particle disintegration in NMC622 cathodes. This study provides important insights into the mechanisms of particle disintegration and capacity fade in NMC/Li-ion batteries, which will enable the design of NMC electrodes that deliver both higher capacities and exhibit better capacity retention.

Original languageEnglish
Pages (from-to)8119-8128
Number of pages10
JournalJournal of Physical Chemistry C
Volume124
Issue number15
DOIs
StatePublished - Apr 16 2020

Fingerprint

Dive into the research topics of 'Probing Sources of Capacity Fade in LiNi0.6Mn0.2Co0.2O2 (NMC622): An Operando XRD Study of Li/NMC622 Batteries during Extended Cycling'. Together they form a unique fingerprint.

Cite this